« Identifying Contributing Degradation Phenomena in PEM Fuel Cell Membrane Electride Assemblies Via Electron Microscopy, Fuel Cell Program: Durability Technical Targets and Testing Protocols The Triple Phase Boundary Platinum electrodeposition for polymer electrolyte membrane fuel cells Kinetic study of the hydrogen oxidation reaction on platinum and Nafion® covered platinum electrodes Electrocatalysis under Conditions of High Mass Transport: Investigation of Hydrogen Oxidation on Single Submicron Pt Particles Supported on Carbon, pp.923-931, 1997. ,
Specificity of the kinetics of H2 evolution to the structure of single-crystal Pt surfaces, and the relation between opd and upd H, Dual-Pathway Kinetic Equation for the Hydrogen Oxidation Reaction on Pt Electrodes Hydrogen oxidation reaction on microelectrodes: Analysis of the contribution of the kinetic routes, pp.1-2, 1998. ,
DOI : 10.1016/S0022-0728(97)00652-9
Kinetics of the Hydrogen Electrode Reaction, Kinetics of the Hydrogen Electrode Reaction, p.1040, 2010. ,
DOI : 10.1246/bcsj.59.725
Density functional theory calculations for the hydrogen evolution reaction in an electrochemical double layer on the Pt(111) electrode, Phys. Chem. Chem. Phys., vol.197, issue.25, pp.25-3241, 2007. ,
DOI : 10.1006/jcat.2000.3087
« RRDE study of oxygen reduction on Pt nanoparticles inside Nafion: H2O2 production in PEMFC cathode conditions, Journal of Applied Electrochemistry, vol.30, issue.7, pp.839-844, 2000. ,
DOI : 10.1023/A:1003999818560
Oxygen Reduction Reaction on Pt and Pt Bimetallic Surfaces: A Selective Review, Fuel Cells, vol.1, issue.2, pp.105-116, 2001. ,
DOI : 10.1002/1615-6854(200107)1:2<105::AID-FUCE105>3.0.CO;2-9
Determination of Catalyst Unique Parameters for the Oxygen Reduction Reaction in a PEMFC, Journal of The Electrochemical Society, vol.46, issue.10, p.1955, 2006. ,
DOI : 10.1149/1.1984351
Study of the Exchange Current Density for the Hydrogen Oxidation and Evolution Reactions, Study of the Exchange Current Density for the Hydrogen Oxidation and Evolution Reactions, p.631, 2007. ,
DOI : 10.1016/0013-4686(64)80088-8
Effect of inert gas flow on hydrogen underpotential deposition measurements in polymer electrolyte fuel cells, Electrochemistry Communications, vol.9, issue.7, pp.1607-1612, 2007. ,
DOI : 10.1016/j.elecom.2007.03.002
Hydrogen sorption ATIN electrodes, Progress in Surface Science, vol.57, issue.2, pp.137-186, 1998. ,
DOI : 10.1016/S0079-6816(98)00015-X
Surface science studies of model fuel cell electrocatalysts, Surface Science Reports, vol.45, issue.4, pp.117-229, 2002. ,
DOI : 10.1016/B978-008044696-7/50051-9
Interfacial processes involving electrocatalytic evolution and oxidation of H2, and the role of chemisorbed H, Electrochimica Acta, vol.47, issue.22-23, pp.22-23, 2002. ,
DOI : 10.1016/S0013-4686(02)00329-8
Electrochemical characterisation of platinum nanoparticles prepared by microemulsion: how to clean them without loss of crystalline surface structure, Journal of Electroanalytical Chemistry, vol.491, issue.1-2, pp.69-77, 2000. ,
DOI : 10.1016/S0022-0728(00)00306-5
Relation of energies and coverages of underpotential and overpotential deposited H at Pt and other metals to the ???volcano curve??? for cathodic H2 evolution kinetics, Electrochimica Acta, vol.45, issue.25-26, pp.25-26, 2000. ,
DOI : 10.1016/S0013-4686(00)00523-5
Oxygen Reduction on Platinum Low-Index Single-Crystal Surfaces in Sulfuric Acid Solution: Rotating Ring-Pt(hkl) Disk Studies, The Journal of Physical Chemistry, vol.99, issue.11, pp.3411-3415, 1995. ,
DOI : 10.1021/j100011a001
Comparison of high surface Pt/C catalysts by cyclic voltammetry, Comparison of high surface Pt/C catalysts by cyclic voltammetry, pp.13-19, 2002. ,
DOI : 10.1016/S0378-7753(01)00921-1
The Impact of Geometric and Surface Electronic Properties of Pt-Catalysts on the Particle Size Effect in Electrocatalysis, The Journal of Physical Chemistry B, vol.109, issue.30, pp.30-14433, 2005. ,
DOI : 10.1021/jp051735z
Active Area Determination of Porous Pt Electrodes Used in Polymer Electrolyte Fuel Cells: Temperature and Humidity Effects, J. Electrochem. Soc, vol.157, pp.12-1795, 2010. ,
Wokaun, « The effect of platinum on carbon corrosion behavior in polymer electrolyte fuel cells, Electrochimica Acta, vol.56, pp.22-7541, 2011. ,
One-dimensional Model of Oxygen Transport Impedance Accounting for Convection Perpendicular to the Electrode, Fuel Cells, vol.162, issue.5, pp.848-861, 2012. ,
DOI : 10.1016/j.jpowsour.2006.06.096
URL : https://hal.archives-ouvertes.fr/hal-01486130
A proton exchange membrane fuel cell impedance model taking into account convection along the air channel: On the bias between the low frequency limit of the impedance and the slope of the polarization curve, Electrochimica Acta, vol.83, pp.13-27, 2012. ,
DOI : 10.1016/j.electacta.2012.07.065
URL : https://hal.archives-ouvertes.fr/hal-01567953
Fuel cell systems for transportation: Status and trends, Journal of Power Sources, vol.177, issue.1, pp.167-176, 2008. ,
DOI : 10.1016/j.jpowsour.2007.10.026
Review: Durability and Degradation Issues of PEM Fuel Cell Components, Fuel Cells, vol.127, issue.446, pp.3-22, 2008. ,
DOI : 10.1016/j.msea.2006.09.098
A review of the main parameters influencing long-term performance and durability of PEM fuel cells, Journal of Power Sources, vol.180, issue.1, pp.1-14, 2008. ,
DOI : 10.1016/j.jpowsour.2008.01.070
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies, Journal of Power Sources, vol.184, issue.1, pp.104-119, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.006
Adroher, « A review of polymer electrolyte membrane fuel cells: Technology, applications, and needs on fundamental research, 2010. ,
Bipolar plates for PEM fuel cells: A review, International Journal of Hydrogen Energy, vol.30, issue.12, pp.1297-1302, 2005. ,
DOI : 10.1016/j.ijhydene.2005.04.016
Corrosion of metal bipolar plates for PEM fuel cells: A review, International Journal of Hydrogen Energy, vol.35, issue.8, pp.3632-3647, 2010. ,
DOI : 10.1016/j.ijhydene.2010.01.059
A comparative study on the corrosion behaviour of 304 austenitic stainless steel in sulfamic and sulfuric acid solutions, Corrosion Science, vol.50, issue.9, pp.2710-2717, 2008. ,
DOI : 10.1016/j.corsci.2008.06.029
Metallic bipolar plates for PEM fuel cells, Metallic bipolar plates for PEM fuel cells, pp.256-260, 2002. ,
DOI : 10.1016/S0378-7753(01)00950-8
Evaluation of the corrosion resistance of Ni???Co???B coatings in simulated PEMFC environment, Electrochimica Acta, vol.51, issue.19, pp.4045-4051, 2006. ,
DOI : 10.1016/j.electacta.2005.11.021
Characteristics of composite bipolar plates for polymer electrolyte membrane fuel cells, Journal of Power Sources, vol.125, issue.2, pp.178-182, 2004. ,
DOI : 10.1016/j.jpowsour.2003.08.039
Combined electrochemical and surface analysis investigation of degradation processes in polymer electrolyte membrane fuel cells, Electrochimica Acta, vol.52, issue.6, pp.2328-2336, 2007. ,
DOI : 10.1016/j.electacta.2006.05.063
XPS investigation of the PTFE induced hydrophobic properties of electrodes for low temperature fuel cells, Applied Surface Science, vol.252, issue.1, pp.148-153, 2005. ,
DOI : 10.1016/j.apsusc.2005.02.007
Model of Carbon Corrosion in PEM Fuel Cells, Journal of The Electrochemical Society, vol.50, issue.8, p.1432, 2006. ,
DOI : 10.1016/0009-2509(56)80014-6
Modeling and Investigation of Design Factors and Their Impact on Carbon Corrosion of PEMFC Electrodes, Journal of The Electrochemical Society, vol.52, issue.7, p.770, 0197. ,
DOI : 10.1149/1.2781015
A Simple Model for Carbon Corrosion in PEM Fuel Cell, Journal of The Electrochemical Society, vol.158, issue.8, p.957, 2011. ,
DOI : 10.1016/S1388-2481(02)00466-6
Carbon support oxidation in PEM fuel cell cathodes, Journal of Power Sources, vol.176, issue.2, pp.444-451, 2008. ,
DOI : 10.1016/j.jpowsour.2007.08.053
A comparative analysis of structural and surface effects in the electrochemical corrosion of carbons, Materials Chemistry and Physics, vol.21, issue.5, pp.495-506, 1989. ,
DOI : 10.1016/0254-0584(89)90148-X
« Formation, microstructural characteristics and stability of carbon supported platinum catalysts for low temperature fuel cells, Journal of Materials Science, vol.38, issue.14, pp.2995-3005, 2003. ,
DOI : 10.1023/A:1024771618027
The role of carbon materials in heterogeneous catalysis, Carbon, vol.36, issue.3, pp.159-175, 1998. ,
DOI : 10.1016/S0008-6223(97)00173-5
Relationship between physicochemical properties and electrooxidation behaviour of carbon materials, Electrochimica Acta, vol.36, issue.13, pp.13-1931, 1991. ,
DOI : 10.1016/0013-4686(91)85075-I
The Effect of Temperature and Pressure on the Performance of a PEMFC Exposed to Transient CO Concentrations, Journal of The Electrochemical Society, vol.3, issue.1, p.29, 2003. ,
DOI : 10.1039/b005843m
Performance Data of a Proton Exchange Membrane Fuel Cell Using H[sub 2]???CO as Fuel Gas, Journal of The Electrochemical Society, vol.143, issue.12, pp.12-3838, 1996. ,
DOI : 10.1149/1.1837305
CO monolayer oxidation on Pt nanoparticles: Further insights into the particle size effects, Journal of Electroanalytical Chemistry, vol.599, issue.2, pp.221-232, 2007. ,
DOI : 10.1016/j.jelechem.2006.02.024
URL : https://hal.archives-ouvertes.fr/hal-00333785
The Effect of the Particle Size on the Kinetics of CO Electrooxidation on High Surface Area Pt Catalysts, Journal of the American Chemical Society, vol.127, issue.18, pp.18-6819, 2005. ,
DOI : 10.1021/ja043602h
Examining a Potential Fuel Cell Poison, Journal of The Electrochemical Society, vol.97, issue.2, p.140, 2002. ,
DOI : 10.1021/j100148a030
Surface Area Loss of Supported Platinum in Polymer Electrolyte Fuel Cells, Journal of The Electrochemical Society, vol.140, issue.10, p.2872, 1993. ,
DOI : 10.1149/1.2220925
Effect of Voltage on Platinum Dissolution, Effect of Voltage on Platinum Dissolution, p.225, 2006. ,
DOI : 10.1149/1.1836156
Instability of Pt???C Electrocatalysts in Proton Exchange Membrane Fuel Cells, Instability of Pt?C Electrocatalysts in Proton Exchange Membrane Fuel Cells, p.2256, 2005. ,
DOI : 10.1007/BF01017860
PEM Fuel Cell Pt???C Dissolution and Deposition in Nafion Electrolyte, Electrochemical and Solid-State Letters, vol.3, issue.5, p.101, 2007. ,
DOI : 10.1149/1.1837307
Membrane Degradation Behavior during Open-Circuit Voltage Hold Test, Journal of The Electrochemical Society, vol.7, issue.8, p.757, 2007. ,
DOI : 10.1149/1.1904988
Bessarabov, « Fingerprint of automotive fuel cell cathode catalyst degradation: Pt band in PEMs, pp.7-10, 2009. ,
Ceramic materials as supports for low-temperature fuel cell catalysts, Solid State Ionics, vol.180, issue.9-10, pp.9-10, 2009. ,
DOI : 10.1016/j.ssi.2009.03.007
Graphitic mesoporous carbon as a durable fuel cell catalyst support, Graphitic mesoporous carbon as a durable fuel cell catalyst support, pp.423-427, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.041
Performance of polymer electrolyte membrane fuel cells with carbon nanotubes as oxygen reduction catalyst support material, Journal of Power Sources, vol.140, issue.2, pp.250-257, 2005. ,
DOI : 10.1016/j.jpowsour.2004.08.042
Alternative supports for the preparation of catalysts for low-temperature fuel cells: the use of carbon nanotubes, Journal of Power Sources, vol.142, issue.1-2, pp.169-176, 2005. ,
DOI : 10.1016/j.jpowsour.2004.10.023
High surface area synthesis, electrochemical activity, and stability of tungsten carbide supported Pt during oxygen reduction in proton exchange membrane fuel cells, Journal of Power Sources, vol.179, issue.1, pp.50-59, 2008. ,
DOI : 10.1016/j.jpowsour.2007.12.105
Stability of platinum based alloy cathode catalysts in PEM fuel cells, Journal of Power Sources, vol.155, issue.2, pp.253-263, 2006. ,
DOI : 10.1016/j.jpowsour.2005.05.011
Heterogeneities of Aging within a PEMFC MEA, Heterogeneities of Aging within a PEMFC MEA, pp.188-198, 2012. ,
DOI : 10.1016/j.jpowsour.2008.03.002
Gold???s future role in fuel cell systems, Journal of Power Sources, vol.118, issue.1-2, pp.1-2, 0199. ,
DOI : 10.1016/S0378-7753(03)00074-0
Synthesis, characterization and application of a Pd/Vulcan and Pd/C catalyst in a PEM fuel cell, International Journal of Hydrogen Energy, vol.29, issue.9, pp.915-920, 2004. ,
DOI : 10.1016/j.ijhydene.2003.06.003
Palladium in fuel cell catalysis, Palladium in fuel cell catalysis, p.915, 2009. ,
DOI : 10.1039/b820837a
Recent development of non-platinum catalysts for oxygen reduction reaction, Journal of Power Sources, vol.152, pp.1-15, 2005. ,
DOI : 10.1016/j.jpowsour.2005.05.098
Easy decoration of carbon nanotubes with well dispersed gold nanoparticles and the use of the material as an electrocatalyst, Carbon, vol.47, issue.4, pp.1146-1151, 2009. ,
DOI : 10.1016/j.carbon.2008.12.049
Solid polymer electrolyte membranes for fuel cell applications???a review, Journal of Membrane Science, vol.259, issue.1-2, pp.10-26, 2005. ,
DOI : 10.1016/j.memsci.2005.01.035
Proton-conducting polymer electrolyte membranes based on hydrocarbon polymers, Progress in Polymer Science, pp.1463-1502, 2000. ,
« Mechanisms of membrane degradation », in in Handbook of Fuel Cells, 2010. ,
Nafion degradation in PEFCs from end plate iron contamination, Electrochimica Acta, vol.48, issue.11, pp.1543-1549, 2003. ,
DOI : 10.1016/S0013-4686(03)00026-4
Phenomenon Analysis of PEFC for Automotive Use(1) Membrane Degradation Behavior During OCV Hold Test, ECS Transactions, pp.519-529, 2006. ,
DOI : 10.1149/1.2356173
Effect of Hydrogen and Oxygen Partial Pressure on Pt Precipitation within the Membrane of PEMFCs, Journal of The Electrochemical Society, vol.14, issue.10, pp.1006-1011, 2007. ,
DOI : 10.1002/fuce.200400050
Advanced materials for improved PEMFC performance and life », Journal of Power Sources, vol.131, pp.1-2, 2004. ,
The effect of humidity on the degradation of Nafion?? membrane, Polymer Degradation and Stability, vol.94, issue.9, pp.1436-1447, 2009. ,
DOI : 10.1016/j.polymdegradstab.2009.05.016
Degradation Mechanism of PEMFC under Open Circuit Operation, Electrochemical and Solid-State Letters, vol.136, issue.137, p.475, 2006. ,
DOI : 10.1021/jp9533382
Gas crossover and membrane degradation in polymer electrolyte fuel cells, Gas crossover and membrane degradation in polymer electrolyte fuel cells, pp.5746-5753, 2006. ,
DOI : 10.1016/j.electacta.2006.03.008
Durability of Perfluorosulfonic Acid and Hydrocarbon Membranes: Effect of Humidity and Temperature, Durability of Perfluorosulfonic Acid and Hydrocarbon Membranes: Effect of Humidity and Temperature », p.119, 2008. ,
DOI : 10.1016/j.jpowsour.2004.01.023
In Situ Analysis of Performance Degradation of a PEMFC under Nonsaturated Humidification, Electrochemical and Solid-State Letters, vol.140, issue.3, p.156, 2005. ,
DOI : 10.1149/1.1854781
Cationic Contamination Effects on Polymer Electrolyte Membrane Fuel Cell Performance, Journal of The Electrochemical Society, vol.11, issue.9, p.1175, 2011. ,
DOI : 10.1016/0013-4686(81)90037-2
Mechanical endurance of polymer electrolyte membrane and PEM fuel cell durability, Journal of Polymer Science Part B: Polymer Physics, vol.138, issue.16, pp.16-2346, 2006. ,
DOI : 10.1016/j.jpowsour.2005.05.011
On mechanical behavior and in-plane modeling of constrained PEM fuel cell membranes subjected to hydration and temperature cycles, Journal of Power Sources, vol.167, issue.2, pp.366-377, 2007. ,
DOI : 10.1016/j.jpowsour.2007.02.025
Measuring the Current Distribution with Submillimeter Resolution in PEFCs, Journal of The Electrochemical Society, vol.156, issue.10, p.1225, 2009. ,
DOI : 10.1016/j.elecom.2005.09.017
Measuring the Current Distribution with Sub-Millimeter Resolution in PEFCs, Journal of The Electrochemical Society, vol.612, issue.3, p.301, 2009. ,
DOI : 10.1016/j.jpowsour.2007.02.025
A Reverse-Current Decay Mechanism for Fuel Cells, Electrochemical and Solid-State Letters, vol.8, issue.6, p.273, 2005. ,
DOI : 10.1149/1.1613669
Transient phenomena in a PEMFC during the start-up of gas feeding observed with a 97-fold segmented cell, Journal of Power Sources, vol.172, issue.1, pp.155-162, 2007. ,
DOI : 10.1016/j.jpowsour.2007.07.062
A multi-instrumented polymer exchange membrane fuel cell: Observation of the in-plane non-homogeneities, Journal of Power Sources, vol.180, issue.2, pp.748-754, 2008. ,
DOI : 10.1016/j.jpowsour.2008.03.002
URL : https://hal.archives-ouvertes.fr/hal-00494964
Study on the processes of start-up and shutdown in proton exchange membrane fuel cells, Journal of Power Sources, vol.189, issue.2, pp.1114-1119, 2009. ,
DOI : 10.1016/j.jpowsour.2008.12.075
Relationship between carbon corrosion and positive electrode potential in a proton-exchange membrane fuel cell during start/stop operation, Journal of Power Sources, vol.192, issue.2, pp.674-678, 2009. ,
DOI : 10.1016/j.jpowsour.2009.03.039
Start/Stop and Local H2 Starvation Mechanisms of Carbon Corrosion: Model vs. Experiment, ECS Transactions, pp.963-973, 2007. ,
DOI : 10.1149/1.2781008
Study of Accelerated Test Protocol for PEFC Focusing on Carbon Corrosion, ECS Transactions, pp.645-655, 2006. ,
DOI : 10.1149/1.2356185
Carbon Corrosion of a PEMFC During Shut-down/Start-up when Using an Air Purge Procedure, ECS Transactions, pp.1301-1311, 2008. ,
DOI : 10.1149/1.2981971
PEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode, Journal of Power Sources, vol.158, issue.2, pp.1306-1312, 2006. ,
DOI : 10.1016/j.jpowsour.2005.10.059
About internal currents during start-up in proton exchange membrane fuel cell, Journal of Power Sources, vol.195, issue.18, pp.5990-5995, 2010. ,
DOI : 10.1016/j.jpowsour.2009.10.093
Start-Stop Phenomena in Channel and Land Areas of a Polymer Electrolyte Fuel Cell, Electrochemical and Solid-State Letters, vol.10, issue.2, p.30, 2011. ,
DOI : 10.1149/1.3148222
Local Catalyst Support Degradation during Polymer Electrolyte Fuel Cell Start-Up and Shutdown, Journal of the Electrochemical Society, vol.159, issue.11, pp.787-793, 2012. ,
DOI : 10.1149/2.019212jes
Understanding and approaches for the durability issues of Pt-based catalysts for PEM fuel cell, Journal of Power Sources, vol.171, issue.2, pp.558-566, 2007. ,
DOI : 10.1016/j.jpowsour.2007.07.004
Carbon supports for low-temperature fuel cell catalysts, Applied Catalysis B: Environmental, vol.88, issue.1-2, pp.1-2, 2009. ,
DOI : 10.1016/j.apcatb.2008.09.030
Aging mechanisms and lifetime of PEFC and DMFC », Journal of Power Sources, vol.127, pp.1-2, 2004. ,
Characterizing the Structural Degradation in a PEMFC Cathode Catalyst Layer: Carbon Corrosion, Journal of The Electrochemical Society, vol.25, issue.8, p.913, 2009. ,
DOI : 10.1016/j.aca.2004.08.005
Platinum dissolution and deposition in the polymer electrolyte membrane of a PEM fuel cell as studied by potential cycling, Phys. Chem. Chem. Phys., vol.29, issue.6, p.746, 2006. ,
DOI : 10.1016/0378-7753(90)85013-3
The Dynamics of Platinum Precipitation in an Ion Exchange Membrane, Journal of The Electrochemical Society, vol.107, issue.3, p.322, 2011. ,
DOI : 10.1016/S0022-0728(01)00698-2
PEM fuel cell electrocatalyst durability measurements, PEM fuel cell electrocatalyst durability measurements, pp.76-81, 2006. ,
DOI : 10.1016/j.jpowsour.2006.03.009
Coarsening of Pt Nanoparticles in Proton Exchange Membrane Fuel Cells upon Potential Cycling, ECS Transactions, pp.185-195, 2006. ,
DOI : 10.1149/1.2214553
Experimental investigation of PEM fuel cell aging under current cycling using segmented fuel cell, International Journal of Hydrogen Energy, vol.35, issue.8, pp.3664-3675, 2010. ,
DOI : 10.1016/j.ijhydene.2010.01.065
Hydrogen and fuel cells: fundamentals, technologies and applications, p.13, 2010. ,
« Electrode degradation mechanisms studies by current distribution measurements Carter, Handbook of Fuel Cells: Fundamentals, Technology and Applications, p.829, 2009. ,
DOI : 10.1002/9780470974001.f500055
« Electrochemical oxide film formation at noble metals as a surfacechemical process, Progress in surface science, pp.331-452, 1995. ,
DOI : 10.1016/0079-6816(95)00040-6
Surface-oxide growth at platinum electrodes in aqueous H2SO4*1Reexamination of its mechanism through combined cyclic-voltammetry, electrochemical quartz-crystal nanobalance, and Auger electron spectroscopy measurements, Electrochimica Acta, vol.49, issue.9-10, pp.9-10, 2004. ,
DOI : 10.1016/S0013-4686(03)00927-7
Kinetic Model of Platinum Dissolution in PEMFCs, Journal of The Electrochemical Society, vol.126, issue.11, p.1523, 2003. ,
DOI : 10.1149/1.2129345
Consumption Rate of Pt under Potential Cycling, Consumption Rate of Pt under Potential Cycling, p.153, 2007. ,
DOI : 10.1149/1.2123638
Physical Theory of Platinum Nanoparticle Dissolution in Polymer Electrolyte Fuel Cells, The Journal of Physical Chemistry C, vol.114, issue.13, pp.5773-5785, 2010. ,
DOI : 10.1021/jp9101509
A surface???electrochemical basis for the direct logarithmic growth law for initial stages of extension of anodic oxide films formed at noble metals, The Journal of Chemical Physics, vol.3, issue.11, p.8361, 1990. ,
DOI : 10.1016/0013-4686(63)85003-3
Lottin, « Internal currents in response to a load change during fuel cell start-up, International Journal of Hydrogen Energy, 2012. ,