A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies, Journal of Power Sources, vol.184, issue.1, p.104, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.006
A review of accelerated stress tests of MEA durability in PEM fuel cells, International Journal of Hydrogen Energy, vol.34, issue.1, p.388, 2009. ,
DOI : 10.1016/j.ijhydene.2008.10.012
The effect of dissolution, migration and precipitation of platinum in Nafion??-based membrane electrode assemblies during fuel cell operation at high potential, Journal of Power Sources, vol.185, issue.2, p.1209, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.098
Polymer Electrolyte Fuel Cell Durability, p.16, 2009. ,
PEM fuel cell relative humidity (RH) and its effect on performance at high temperatures, Electrochimica Acta, vol.53, issue.16, p.5315, 2008. ,
DOI : 10.1016/j.electacta.2008.02.074
PEM fuel cell electrocatalyst durability measurements, Journal of Power Sources, vol.163, issue.1, p.76, 2006. ,
DOI : 10.1016/j.jpowsour.2006.03.009
The effect of humidity and oxygen partial pressure on degradation of Pt/C catalyst in PEM fuel cell, Electrochimica Acta, vol.54, issue.6, p.1826, 2009. ,
DOI : 10.1016/j.electacta.2008.10.008
Membrane electrode assembly degradation by dry/wet gas on a PEM fuel cell, International Journal of Hydrogen Energy, vol.35, issue.23, p.13125, 2010. ,
DOI : 10.1016/j.ijhydene.2010.04.077
Diagnosis of MEA degradation under accelerated relative humidity cycling, Journal of Power Sources, vol.196, issue.11, p.5045, 2011. ,
DOI : 10.1016/j.jpowsour.2011.01.088
Degradation on a PTFE/Nafion membrane electrode assembly with accelerating degradation technique, International Journal of Hydrogen Energy, vol.35, issue.13, p.6941, 2010. ,
DOI : 10.1016/j.ijhydene.2010.03.118
Effects of Ozone on the Performance of a Polymer Electrolyte Membrane Fuel Cell, Fuel Cells, vol.154, issue.5, p.562, 2009. ,
DOI : 10.1002/fuce.200800182
URL : https://hal.archives-ouvertes.fr/hal-00508342
Real surface area measurements in electrochemistry, Journal of Electroanalytical Chemistry, vol.327, issue.1-2, p.353, 1992. ,
DOI : 10.1016/0022-0728(92)80162-W
Magnetic resonance imaging of water distribution and production in a 6cm2 PEMFC under operation, International Journal of Hydrogen Energy, vol.33, issue.12, p.3146, 2008. ,
DOI : 10.1016/j.ijhydene.2008.01.053
URL : https://hal.archives-ouvertes.fr/hal-00298490
A review of PEM hydrogen fuel cell contamination: Impacts, mechanisms, and mitigation, Journal of Power Sources, vol.165, issue.2, p.739, 2007. ,
DOI : 10.1016/j.jpowsour.2006.12.012
PEM fuel cell relative humidity (RH) and its effect on performance at high temperatures, Electrochimica Acta, vol.53, issue.16, p.5315, 2008. ,
DOI : 10.1016/j.electacta.2008.02.074
Polymer Electrolyte Fuel Cell Durability, Chap, vol.3, p.60, 2009. ,
Characterization of Flemion?? membranes for PEFC, Electrochimica Acta, vol.43, issue.24, p.3749, 1998. ,
DOI : 10.1016/S0013-4686(98)00133-9
Nafion/PTFE composite membranes for fuel cell applications, Journal of Membrane Science, vol.212, issue.1-2, p.213, 2003. ,
DOI : 10.1016/S0376-7388(02)00503-3
Effect of gas composition on Ru dissolution and crossover in polymer-electrolyte membrane fuel cells, Journal of Power Sources, vol.195, issue.15, p.4622, 2010. ,
DOI : 10.1016/j.jpowsour.2010.02.028
Investigation of MEA degradation in PEM fuel cell by on/off cyclic operation under different humid conditions, International Journal of Hydrogen Energy, vol.36, issue.2, p.1828, 2011. ,
DOI : 10.1016/j.ijhydene.2010.02.053
The corrosion of PEM fuel cell catalyst supports and its implications for developing durable catalysts, Electrochimica Acta, vol.54, issue.11, p.3109, 2009. ,
DOI : 10.1016/j.electacta.2008.12.001
Surface oxidation of carbon supports due to potential cycling under PEM fuel cell conditions, Electrochimica Acta, vol.55, issue.16, p.4765, 2010. ,
DOI : 10.1016/j.electacta.2010.03.056
PEM fuel cell relative humidity (RH) and its effect on performance at high temperatures, Electrochimica Acta, vol.53, issue.16, p.5315, 2008. ,
DOI : 10.1016/j.electacta.2008.02.074
Water transport in the proton exchange-membrane fuel cell: Comparison of model computation and measurements of effective drag, Journal of Power Sources, vol.162, issue.2, p.1130, 2006. ,
DOI : 10.1016/j.jpowsour.2006.07.043
Characterization of Flemion?? membranes for PEFC, Electrochimica Acta, vol.43, issue.24, p.3749, 1998. ,
DOI : 10.1016/S0013-4686(98)00133-9
Nafion/PTFE composite membranes for fuel cell applications, Journal of Membrane Science, vol.212, issue.1-2, p.213, 2003. ,
DOI : 10.1016/S0376-7388(02)00503-3
Degradation mechanism study of perfluorinated proton exchange membrane under fuel cell operating conditions, Electrochimica Acta, vol.53, issue.8, p.3279, 2008. ,
DOI : 10.1016/j.electacta.2007.11.010
Diagnosis of MEA degradation under accelerated relative humidity cycling, Journal of Power Sources, vol.196, issue.11, p.5045, 2011. ,
DOI : 10.1016/j.jpowsour.2011.01.088
Aging mechanisms and lifetime of PEFC and DMFC, Journal of Power Sources, vol.127, issue.1-2, p.127, 2004. ,
DOI : 10.1016/j.jpowsour.2003.09.033
Effects of Ozone on the Performance of a Polymer Electrolyte Membrane Fuel Cell, Fuel Cells, vol.154, issue.5, p.562, 2009. ,
DOI : 10.1002/fuce.200800182
URL : https://hal.archives-ouvertes.fr/hal-00508342
Ageing of PEMFC???s due to operation at low current density: Investigation of oxidative degradation, International Journal of Hydrogen Energy, vol.35, issue.19, p.10472, 2010. ,
DOI : 10.1016/j.ijhydene.2010.07.180
Analysis of proton exchange membrane fuel cell polarization losses at elevated temperature 120??C and reduced relative humidity, Electrochimica Acta, vol.52, issue.11, p.3525, 2007. ,
DOI : 10.1016/j.electacta.2006.10.015
Exploring the effects of symmetrical and asymmetrical relative humidity on the performance of H2/air PEM fuel cell at different temperatures, Journal of Power Sources, vol.164, issue.2, p.503, 2007. ,
DOI : 10.1016/j.jpowsour.2006.11.065
PEM fuel cell electrocatalyst durability measurements, Journal of Power Sources, vol.163, issue.1, p.76, 2006. ,
DOI : 10.1016/j.jpowsour.2006.03.009
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies, Journal of Power Sources, vol.184, issue.1, p.104, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.006
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation, Chemical Reviews, vol.107, issue.10, p.3904, 2007. ,
DOI : 10.1021/cr050182l
A review of accelerated stress tests of MEA durability in PEM fuel cells, International Journal of Hydrogen Energy, vol.34, issue.1, p.388, 2009. ,
DOI : 10.1016/j.ijhydene.2008.10.012
Investigation of thermal and electrochemical degradation of fuel cell catalysts, Journal of Power Sources, vol.160, issue.2, p.977, 2006. ,
DOI : 10.1016/j.jpowsour.2006.03.033
The corrosion of PEM fuel cell catalyst supports and its implications for developing durable catalysts, Electrochimica Acta, vol.54, issue.11, p.3109, 2009. ,
DOI : 10.1016/j.electacta.2008.12.001
Surface oxidation of carbon supports due to potential cycling under PEM fuel cell conditions, Electrochimica Acta, vol.55, issue.16, p.4765, 2010. ,
DOI : 10.1016/j.electacta.2010.03.056
The effect of humidity and oxygen partial pressure on degradation of Pt/C catalyst in PEM fuel cell, Electrochimica Acta, vol.54, issue.6, p.1826, 2009. ,
DOI : 10.1016/j.electacta.2008.10.008
Heat-Treated Carbon-Blacks as Supports for Platinum Catalysts, Journal of Catalysis, vol.154, issue.2, p.299, 1995. ,
DOI : 10.1006/jcat.1995.1171
Polymer Electrolyte Fuel Cell Durability, p.190, 2009. ,
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation, Chemical Reviews, vol.107, issue.10, pp.3904-51, 2007. ,
DOI : 10.1021/cr050182l
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies, Journal of Power Sources, vol.184, issue.1, pp.104-123, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.006
A review of accelerated stress tests of MEA durability in PEM fuel cells, International Journal of Hydrogen Energy, vol.34, issue.1, pp.388-404, 2009. ,
DOI : 10.1016/j.ijhydene.2008.10.012
Degradation of polymer electrolyte membranes, International Journal of Hydrogen Energy, vol.31, issue.13, pp.1838-54, 2006. ,
DOI : 10.1016/j.ijhydene.2006.05.006
The effects of pinholes on proton exchange membrane fuel cell performance, International Journal of Energy Research, vol.150, issue.1, pp.24-30, 2011. ,
DOI : 10.1002/er.1728
Diagnosis of MEA degradation under accelerated relative humidity cycling, Journal of Power Sources, vol.196, issue.11, pp.5045-52, 2011. ,
DOI : 10.1016/j.jpowsour.2011.01.088
Accelerated durability testing via reactants relative humidity cycling on PEM fuel cells Applied Energy ,
Gas crossover and membrane degradation in polymer electrolyte fuel cells, Electrochimica Acta, vol.51, issue.26, pp.5746-53, 2006. ,
DOI : 10.1016/j.electacta.2006.03.008
Characterization of gas crossover and its implications in PEM fuel cells, AIChE Journal, vol.3, issue.6, 2006. ,
DOI : 10.1002/aic.10780
Membrane and Active Layer Degradation upon PEMFC Steady-State Operation, Journal of The Electrochemical Society, vol.14, issue.11, pp.1106-1120, 2007. ,
DOI : 10.1149/1.2266163
URL : https://hal.archives-ouvertes.fr/hal-00386380
Diagnostic tools in PEM fuel cell research: Part I Electrochemical techniques, International Journal of Hydrogen Energy, vol.33, issue.6, pp.1735-1781, 2008. ,
DOI : 10.1016/j.ijhydene.2008.01.013
Real surface area measurements in electrochemistry, Journal of Electroanalytical Chemistry, vol.327, issue.1-2, pp.353-76, 1992. ,
DOI : 10.1016/0022-0728(92)80162-W
Experimental study on water transport coefficient in Proton Exchange Membrane Fuel Cell, Journal of Power Sources, vol.190, issue.2, pp.230-270, 2009. ,
DOI : 10.1016/j.jpowsour.2009.01.038
URL : https://hal.archives-ouvertes.fr/hal-00494463
PEM fuel cell relative humidity (RH) and its effect on performance at high temperatures, Electrochimica Acta, vol.53, issue.16, pp.5315-5336, 2008. ,
DOI : 10.1016/j.electacta.2008.02.074
Analysis of proton exchange membrane fuel cell polarization losses at elevated temperature 120??C and reduced relative humidity, Electrochimica Acta, vol.52, issue.11, pp.3525-3558, 2007. ,
DOI : 10.1016/j.electacta.2006.10.015
Influence of temperature and relative humidity on performance and CO tolerance of PEM fuel cells with Nafion?????Teflon?????Zr(HPO4)2 higher temperature composite membranes, Electrochimica Acta, vol.51, issue.26, pp.5596-605, 2006. ,
DOI : 10.1016/j.electacta.2006.02.033
Experimental Investigation of Air Relative Humidity (RH) Cycling Tests on MEA/Cell Aging in PEMFC Part I: Study of High RH Cycling Test With air RH at 62%/100%, Fuel Cells, vol.155, issue.3, pp.335-381, 2012. ,
DOI : 10.1016/j.electacta.2010.03.056
URL : https://hal.archives-ouvertes.fr/hal-00778278
Experimental Investigation of Air Relative Humidity (RH) Cycling Tests on MEA/Cell Aging in PEMFC Part II: Study of Low RH Cycling Test with Air RH at 62%/0%, Fuel Cells, vol.154, issue.3, pp.347-55, 2012. ,
DOI : 10.1006/jcat.1995.1171
URL : https://hal.archives-ouvertes.fr/hal-00778279
Effects of Ozone on the Performance of a Polymer Electrolyte Membrane Fuel Cell, Fuel Cells, vol.154, issue.5, pp.562-571, 2009. ,
DOI : 10.1002/fuce.200800182
URL : https://hal.archives-ouvertes.fr/hal-00508342
Hybrid artificial bee colony algorithm for parameter estimation of proton exchange membrane fuel cell, International Journal of Hydrogen Energy, vol.38, issue.14, pp.5796-5806, 2013. ,
DOI : 10.1016/j.ijhydene.2013.01.058
Fuel cells for non-automotive uses: Status and prospects, International Journal of Hydrogen Energy, vol.37, issue.8, pp.6339-6348, 2012. ,
DOI : 10.1016/j.ijhydene.2012.01.060
Production of hydrogen from renewable resources and its effectiveness, International Journal of Hydrogen Energy, vol.37, issue.16, pp.11563-11578, 2012. ,
DOI : 10.1016/j.ijhydene.2012.05.047
A figure of merit assessment of the routes to hydrogen, International Journal of Hydrogen Energy, vol.30, issue.8, pp.809-819, 2005. ,
DOI : 10.1016/j.ijhydene.2005.02.003
Platinum-Alloy Cathode Catalyst Degradation in Proton Exchange Membrane Fuel Cells: Nanometer-Scale Compositional and Morphological Changes, Journal of The Electrochemical Society, vol.157, issue.1, p.82, 2010. ,
DOI : 10.1063/1.2948902
Gas crossover and membrane degradation in polymer electrolyte fuel cells, Electrochimica Acta, vol.51, issue.26, pp.5746-5753, 2006. ,
DOI : 10.1016/j.electacta.2006.03.008
Gas Permeation Properties of Solid Polymer Electrolyte (SPE) Membranes, Journal of The Electrochemical Society, vol.132, issue.6, pp.1328-1332, 1985. ,
DOI : 10.1149/1.2114111
Gas Permeation in SPE Method, Journal of The Electrochemical Society, vol.131, issue.4, pp.769-773, 1984. ,
DOI : 10.1149/1.2115696
Studies of perfluorinated ion exchange membranes for polymer electrolyte fuel cells, Denki Kagaku, vol.64, issue.6, pp.727-736, 1996. ,
Characterization of gas crossover and its implications in PEM fuel cells, AIChE Journal, vol.3, issue.6, pp.1916-1925, 2006. ,
DOI : 10.1002/aic.10780
Recent advances in perfluorinated ionomer membranes: structure, properties and applications, Journal of Membrane Science, vol.120, issue.1, pp.1-33, 1996. ,
DOI : 10.1016/0376-7388(96)00155-X
Small-Angle Scattering Study of Short Pendant Chain Perfuorosulfonated Ionomer Membranes, Macromolecules, vol.33, issue.13, pp.4850-4855, 2000. ,
DOI : 10.1021/ma9912709
Elaboration d'électrodes de pile à combustible par plasma, Thèse de doctorat, 2006. ,
Dependence of PEM fuel cell performance on catalyst loading, Journal of Power Sources, vol.127, issue.1-2, pp.1-2, 2004. ,
DOI : 10.1016/j.jpowsour.2003.09.013
Analysis and Evaluation of Aging Phenomena in PEMFCs, Advances in Chemical Engineering, vol.41, pp.265-330, 2012. ,
DOI : 10.1016/B978-0-12-386874-9.00009-9
Electrocatalytic Corrosion of Carbon Support in PEMFC Cathodes, Electrochemical and Solid-State Letters, vol.97, issue.1, pp.19-22, 2004. ,
DOI : 10.1021/j100148a030
Activity benchmarks and requirements for Pt, Pt-alloy, and non-Pt oxygen reduction catalysts for PEMFCs, Applied Catalysis B: Environmental, vol.56, issue.1-2, pp.1-2, 2005. ,
DOI : 10.1016/j.apcatb.2004.06.021
Nanostructured Coral-like Carbon as Pt Support for Fuel Cells, The Journal of Physical Chemistry C, vol.114, issue.15, pp.6976-6982, 2010. ,
DOI : 10.1021/jp100397h
Dealloyed Pt-Cu Core-Shell Nanoparticle Electrocatalysts for Use in PEM, Fuel Cell Cathodes, vol.112, issue.7, pp.2770-2778, 2008. ,
Co Alloy Surfaces, The Journal of Physical Chemistry B, vol.106, issue.46, pp.11970-11979, 2002. ,
DOI : 10.1021/jp021182h
Dealloyed binary PtM 3 (M=Cu, Co, Ni) and ternary PtNi 3 M (M=Cu, Co, Fe, Cr) electrocatalysts for the oxygen reduction reaction: Performance in polymer electrolyte membrane fuel cells, pp.666-673, 2011. ,
Surface Strain versus Substrate Interaction in Heteroepitaxial Metal Layers: Pt on Ru(0001), Physical Review Letters, vol.46, issue.1, p.16101, 2003. ,
DOI : 10.1023/A:1019073208575
Further insights into the durability of Pt3Co/C electrocatalysts: Formation of ???hollow??? Pt nanoparticles induced by the Kirkendall effect, Electrochimica Acta, vol.56, issue.28, pp.10658-10667, 2011. ,
DOI : 10.1016/j.electacta.2011.03.073
Impact of metal cations on the electrocatalytic properties of Pt/C nanoparticles at multiple phase interfaces, Physical Chemistry Chemical Physics, vol.106, issue.37, p.13000, 2012. ,
DOI : 10.1021/jp013195l
Non precious metal catalysts for the PEM fuel cell cathode, International Journal of Hydrogen Energy, vol.37, issue.1, pp.357-372, 2012. ,
DOI : 10.1016/j.ijhydene.2011.08.095
Electrochemical study of Pt?Pd, Pt?Ru, Pt?Rh and Pt?Sn/C in acid media for hydrogen adsorption?desorption reaction, Journal of Alloys and Compounds, pp.434-435, 2007. ,
Electrocatalysis by ad-atoms, Journal of Electroanalytical Chemistry and Interfacial Electrochemistry, vol.60, issue.3, pp.267-273, 1975. ,
DOI : 10.1016/S0022-0728(75)80261-0
Gas diffusion layer for proton exchange membrane fuel cells???A review, Journal of Power Sources, vol.194, issue.1, pp.146-160, 2009. ,
DOI : 10.1016/j.jpowsour.2009.04.005
A Review of Water Management in Polymer Electrolyte Membrane Fuel Cells, Energies, vol.1, issue.4, pp.1057-1106, 2009. ,
DOI : 10.1016/j.ijhydene.2009.01.071
A review of gas diffusion layer in PEM fuel cells: Materials and designs, International Journal of Hydrogen Energy, vol.37, issue.7, pp.5850-5865, 2012. ,
DOI : 10.1016/j.ijhydene.2011.12.148
Microporous layer for water morphology control in PEMFC, International Journal of Heat and Mass Transfer, vol.52, issue.11-12, pp.11-12, 2009. ,
DOI : 10.1016/j.ijheatmasstransfer.2009.01.002
Review: Durability and Degradation Issues of PEM Fuel Cell Components, Fuel Cells, vol.127, issue.446, pp.3-22, 2008. ,
DOI : 10.1016/j.msea.2006.09.098
Design analysis of PEMFC bipolar plates considering stack manufacturing and environment impact, Journal of Power Sources, vol.129, issue.2, pp.152-169, 2004. ,
DOI : 10.1016/j.jpowsour.2003.11.037
Use of stainless steel for cost competitive bipolar plates in the SPFC, Journal of Power Sources, vol.86, issue.1-2, pp.274-282, 2000. ,
DOI : 10.1016/S0378-7753(99)00460-7
Bipolar plate materials for solid polymer fuel cells, Journal of Applied Electrochemistry, vol.30, issue.1, pp.101-105, 2000. ,
DOI : 10.1023/A:1003831406406
Flow distribution in proton exchange membrane fuel cell stacks, Journal of Power Sources, vol.162, issue.1, pp.340-355, 2006. ,
DOI : 10.1016/j.jpowsour.2006.06.081
Heterogeneous Cell Ageing in Polymer Electrolyte Fuel Cell Stacks, Polymer Electrolyte Fuel Cell Durability, pp.431-439, 2009. ,
DOI : 10.1007/978-0-387-85536-3_22
Design of an 80kWe PEM fuel cell system: Scale up effect investigation, Journal of Power Sources, vol.182, issue.2, pp.441-448, 2008. ,
DOI : 10.1016/j.jpowsour.2007.12.100
URL : https://hal.archives-ouvertes.fr/hal-00377532
Comparative studies of polymer electrolyte membrane fuel cell stack and single cell, Journal of Power Sources, vol.80, pp.1-2, 1999. ,
Effect of operative conditions on a PEFC stack performance, International Journal of Hydrogen Energy, vol.33, issue.12, pp.3137-3141, 2008. ,
DOI : 10.1016/j.ijhydene.2007.11.014
Design, assembly and operation of polymer electrolyte membrane fuel cell stacks to 1 kWe capacity, Journal of Power Sources, vol.125, issue.2, pp.155-165, 2004. ,
DOI : 10.1016/j.jpowsour.2003.08.026
Operational aspects of a large PEFC stack under practical conditions, Journal of Power Sources, vol.128, issue.2, pp.208-217, 2004. ,
DOI : 10.1016/j.jpowsour.2003.09.060
Uniformity analysis at MEA and stack Levels for a Nexa PEM fuel cell system, Journal of Power Sources, vol.128, issue.2, pp.231-238, 2004. ,
DOI : 10.1016/j.jpowsour.2003.09.074
/PBI Celtec-P MEAs for ??-CHP Applications, Fuel Cells, vol.172, issue.4, pp.325-348, 2009. ,
DOI : 10.1002/fuce.200800134
PEM fuel cell testing by electrochemical impedance spectroscopy, Electric Power Systems Research, vol.79, issue.1, pp.17-26, 2009. ,
DOI : 10.1016/j.epsr.2008.05.012
Thermal management issues in a PEMFC stack ??? A brief review of current status, Applied Thermal Engineering, vol.29, issue.7, pp.1276-1280, 2009. ,
DOI : 10.1016/j.applthermaleng.2008.05.009
Analysis of a PEMFC durability test under low humidity conditions and stack behaviour modelling using experimental design techniques, Journal of Power Sources, vol.182, issue.2, pp.429-440, 2008. ,
DOI : 10.1016/j.jpowsour.2007.12.122
URL : https://hal.archives-ouvertes.fr/hal-00413859
Performance investigation of 2.4kW PEM fuel cell stack in vehicles, International Journal of Hydrogen Energy, vol.32, issue.17, pp.4340-4349, 2007. ,
DOI : 10.1016/j.ijhydene.2007.05.043
Comparison between two PEM fuel cell durability tests performed at constant current and under solicitations linked to transport mission profile, International Journal of Hydrogen Energy, vol.32, issue.17, pp.4523-4536, 2007. ,
DOI : 10.1016/j.ijhydene.2007.03.013
URL : https://hal.archives-ouvertes.fr/hal-00503003
/PBI Celtec-P Based Membrane Electrode Assemblies for Micro-CHP Applications, Fuel Cells, vol.33, issue.2, pp.299-311, 2010. ,
DOI : 10.1002/fuce.200900153
Impedance Measurement of Each Cell of a 10 W PEMFC Stack under Load, Journal of The Electrochemical Society, vol.70, issue.12, p.2193, 2004. ,
DOI : 10.1149/1.1815152
URL : https://hal.archives-ouvertes.fr/hal-00417921
PEM Fuel Cells, 2005. ,
DOI : 10.1007/1-84628-207-1_2
Hydrogen-fed PEMFC: Overvoltage analysis during an activation procedure, Journal of Electroanalytical Chemistry, vol.671, pp.58-66, 2012. ,
DOI : 10.1016/j.jelechem.2012.02.013
Oxygen Reduction on Oxide-Free Platinum in 85%Orthophosphoric Acid: Temperature and Impurity Dependence, Journal of The Electrochemical Society, vol.117, issue.3, pp.328-335, 1970. ,
DOI : 10.1149/1.2407503
Mécanismes de vieillissement d'assemblage membrane-électrodes dans une pile à combustible de type PEM par approche expérimentale, Thèse de doctorat, 2012. ,
Long-term durability study of perfluoropolymer membranes in low humidification conditions, Journal of Solid State Electrochemistry, vol.168, issue.3, pp.1209-1216, 2010. ,
DOI : 10.1016/j.ssi.2003.01.001
Membrane electrode assembly degradation by dry/wet gas on a PEM fuel cell, International Journal of Hydrogen Energy, vol.35, issue.23, pp.13125-13130, 2010. ,
DOI : 10.1016/j.ijhydene.2010.04.077
A review of polymer electrolyte membrane fuel cell durability test protocols, Journal of Power Sources, vol.196, issue.22, pp.9107-9116, 2011. ,
DOI : 10.1016/j.jpowsour.2011.07.082
Experimental investigation of pinhole effect on MEA/cell aging in PEMFC, International Journal of Hydrogen Energy, vol.38, issue.1, pp.543-550, 2013. ,
DOI : 10.1016/j.ijhydene.2012.09.058
Experimental Investigation of Air Relative Humidity (RH) Cycling Tests on MEA/Cell Aging in PEMFC Part I: Study of High RH Cycling Test With air RH at 62%/100%, Fuel Cells, vol.155, issue.3, pp.100-112, 2012. ,
DOI : 10.1016/j.electacta.2010.03.056
URL : https://hal.archives-ouvertes.fr/hal-00778278
Experimental Investigation of Air Relative Humidity (RH) Cycling Tests on MEA/Cell Aging in PEMFC Part II: Study of Low RH Cycling Test with Air RH at 62%/0%, Fuel Cells, vol.154, issue.3, pp.347-355, 2012. ,
DOI : 10.1006/jcat.1995.1171
URL : https://hal.archives-ouvertes.fr/hal-00778279
Impact of gas stoichiometry on water management and fuel cell performance of a sulfonated Poly(Ether Ether Ketone) membrane, Journal of Power Sources, vol.206, pp.161-170, 2012. ,
DOI : 10.1016/j.jpowsour.2012.01.102
Characterisation of proton exchange membrane fuel cell (PEMFC) failures via electrochemical impedance spectroscopy, Journal of Power Sources, vol.161, issue.1, pp.264-274, 2006. ,
DOI : 10.1016/j.jpowsour.2006.03.067
Impedance-based diagnosis of polymer electrolyte membrane fuel cell failures associated with a low frequency ripple current, Renewable Energy, vol.51, pp.51-302, 2013. ,
DOI : 10.1016/j.renene.2012.09.053
Impedance study of membrane dehydration and compression in proton exchange membrane fuel cells, Journal of Power Sources, vol.192, issue.2, pp.457-466, 2009. ,
DOI : 10.1016/j.jpowsour.2009.03.027
Modelisticinterpretation of the impedance response of a polymer electrolyte fuel cell, Electrochimica Acta, vol.43, issue.24, pp.3761-3766, 1998. ,
DOI : 10.1016/S0013-4686(98)00135-2
Optimal composition of polymer electrolyte fuel cell electrodes determined by the AC impedance method, Journal of Power Sources, vol.94, issue.1, pp.78-84, 2001. ,
DOI : 10.1016/S0378-7753(00)00629-7
Influence of Nafion loading in the catalyst layer of gas-diffusion electrodes for PEFC, Journal of Power Sources, vol.77, issue.2, pp.136-142, 1999. ,
DOI : 10.1016/S0378-7753(98)00186-4
Electrical test methods for on-line fuel cell ohmic resistance measurement, Journal of Power Sources, vol.160, issue.2, pp.1088-1095, 2006. ,
DOI : 10.1016/j.jpowsour.2006.02.086
Real surface area measurements in electrochemistry, Journal of Electroanalytical Chemistry, vol.327, issue.1-2, pp.353-376, 1992. ,
DOI : 10.1016/0022-0728(92)80162-W
Structure of dealloyed PtCu thin films and catalytic activity for oxygen reduction, pp.22-4712, 2010. ,
Degradation study of Pt-based alloy catalysts for the oxygen reduction reaction in proton exchange membrane fuel cells, Journal of Electroanalytical Chemistry, vol.648, issue.2, pp.156-162, 2010. ,
DOI : 10.1016/j.jelechem.2010.07.013
The effect of ambient contamination on PEMFC performance, Journal of Power Sources, vol.166, issue.1, pp.172-176, 2007. ,
DOI : 10.1016/j.jpowsour.2006.12.103
Comparative analysis of the electroactive area of Pt/C PEMFC electrodes in liquid and solid polymer contact by underpotential hydrogen adsorption/desorption, International Journal of Hydrogen Energy, vol.34, issue.11, pp.4838-4846, 2009. ,
DOI : 10.1016/j.ijhydene.2009.03.053
Studies of performance decay of Pt/C catalysts with working time of proton exchange membrane fuel cell, Journal of Power Sources, vol.184, issue.1, pp.245-250, 2008. ,
DOI : 10.1016/j.jpowsour.2008.06.037
Comparison of high surface Pt/C catalysts by cyclic voltammetry, Journal of Power Sources, vol.105, issue.1, pp.13-19, 2002. ,
DOI : 10.1016/S0378-7753(01)00921-1
Electrochemical characterisation of Pt/C suspensions for the reduction of oxygen, Journal of Power Sources, vol.151, pp.2-10, 2005. ,
DOI : 10.1016/j.jpowsour.2005.02.077
Development of new test instruments and protocols for the diagnostic of fuel cell stacks, Journal of Power Sources, vol.196, issue.12, pp.5325-5333, 2011. ,
DOI : 10.1016/j.jpowsour.2010.08.029
URL : https://hal.archives-ouvertes.fr/hal-01006663
Electrochemical Characterization of the Active Surface in Carbon-Supported Platinum Electrocatalysts for PEM Fuel Cells, Journal of The Electrochemical Society, vol.109, issue.6, p.770, 2003. ,
DOI : 10.1016/S0378-7753(02)00238-0
Development of a galvanostatic analysis technique as an in-situ diagnostic tool for PEMFC single cells and stacks, International Journal of Hydrogen Energy, vol.37, issue.7, pp.5891-5900, 2012. ,
DOI : 10.1016/j.ijhydene.2011.12.152
Measurement of ohmic voltage losses in individual cells of a PEMFC stack, Journal of Power Sources, vol.112, issue.1, pp.261-272, 2002. ,
DOI : 10.1016/S0378-7753(02)00391-9
AC impedance diagnosis of a 500W PEM fuel cell stack, Journal of Power Sources, vol.161, issue.2, pp.920-928, 2006. ,
DOI : 10.1016/j.jpowsour.2006.05.003
A review on PEM voltage degradation associated with water management: Impacts, influent factors and characterization, Journal of Power Sources, vol.183, issue.1, pp.260-274, 2008. ,
DOI : 10.1016/j.jpowsour.2008.04.037
AC impedance characteristics of a 2kW PEM fuel cell stack under different operating conditions and load changes, International Journal of Hydrogen Energy, vol.32, issue.17, pp.4358-4364, 2007. ,
DOI : 10.1016/j.ijhydene.2007.06.024
A polymer electrolyte fuel cell life test: 3 years of continuous operation, Journal of Power Sources, vol.158, issue.1, pp.446-454, 2006. ,
DOI : 10.1016/j.jpowsour.2005.09.062
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation, Scientific aspects of polymer electrolyte fuel cell durability and degradation, pp.3904-3951, 2007. ,
DOI : 10.1021/cr050182l
Development and performance of a 10kW PEMFC stack, Journal of Power Sources, vol.127, issue.1-2, pp.206-212, 2004. ,
DOI : 10.1016/j.jpowsour.2003.09.040
Longevity test results for reformate polymer electrolyte membrane fuel cell stacks, Journal of Power Sources, vol.196, issue.12, pp.5264-5271, 2011. ,
DOI : 10.1016/j.jpowsour.2010.08.113
Investigation of solid oxide fuel cell short stacks for mobile applications by electrochemical impedance spectroscopy, Electrochimica Acta, vol.53, issue.25, pp.7509-7513, 2008. ,
DOI : 10.1016/j.electacta.2008.04.047
Characterisation and Modelling of a High Temperature PEM Fuel Cell Stack using Electrochemical Impedance Spectroscopy, Fuel Cells, vol.168, issue.4, pp.463-473, 2009. ,
DOI : 10.1002/fuce.200800137
A review of accelerated conditioning for a polymer electrolyte membrane fuel cell 196, pp.9097-9106, 2011. ,
Gas-Crossover and Membrane-Pinhole Effects in Polymer-Electrolyte Fuel Cells, Journal of The Electrochemical Society, vol.52, issue.6, p.521, 2008. ,
DOI : 10.1149/1.1855871
Investigation of Membrane Pinhole Effects in Polymer Electrolyte Fuel Cells by Locally Resolved Current Density, Journal of The Electrochemical Society, vol.158, issue.1, p.11, 2011. ,
DOI : 10.1016/j.ijhydene.2008.10.054
Application of a segmented cell setup to detect pinhole and catalyst loading defects in proton exchange membrane fuel cells, Electrochimica Acta, vol.76, pp.76-92, 2012. ,
DOI : 10.1016/j.electacta.2012.04.138
Factors determining the gas crossover through pinholes in polymer electrolyte fuel cell membranes, Electrochimica Acta, vol.80, pp.240-247, 2012. ,
DOI : 10.1016/j.electacta.2012.07.013
AC impedance diagnosis of a 500W PEM fuel cell stack, Journal of Power Sources, vol.161, issue.2, pp.929-937, 2006. ,
DOI : 10.1016/j.jpowsour.2006.07.020
Mathematics of statistics, 1964. ,
A) maturation d'Ostwald, (B) précipitation du Pt dans le ionomère, et (C) coalescence des particules de Pt, p.16 ,
évolution de la morphologie et de la composition d'un catalyseur cathodique de Pt-Co provoquée par une lixiviation acide et un cyclage en potentiel ,
Face externe (gauche) et face interne (droite), p.31 ,
et de Nyquist (droite) d'une cellule de 100 cm (10 kHz-100 mHz, courant imposé de 0,3 A.cm -2 avec une perturbation de 10% d'amplitude du signal), p.41 ,
Pinhole " ainsi que des cellules individuelles en début de test, p.85 ,
Résistance ohmique (gauche) et résistance de transfert de charge (droite) de la monocellule référence et des cellules du stack " Pinhole, p.85 ,
30 mV.s -1 ) des cellules du stack " Pinhole " en fin de test, p.88 ,
2 mV.s -1 ) des cellules du stack " Pinhole " en fin de test, p.89 ,
2 mV.s -1 ) de la monocellule défectueuse (stack DEF) en début et fin de test, p.102 ,